PA6 | 聚已内酰胺#尼龙6
泰国宇部
规格级别: 挤出 备注说明: 特性:高粘度 1030B 物性表| 基本性能 | 额定值 | 单位 | 测试方法 |
|---|---|---|---|
| 吸水率 | 10.7 | % | ASTM D-570 |
| 成型收缩率 | 1.2 | % | UBEmethod |
| 吸水率 | 1.8 | % | ASTM D-570 |
| 物理性能 | 额定值 | 单位 | 测试方法 |
|---|---|---|---|
| 比重 | 1.14 | ASTM D-792 | |
| 薄雾 | 3 | % | |
| 光泽 | 140 | % | |
| 薄膜厚度 | 50 | μm | |
| 静态磨擦 | 1.0 |
| 机械性能 | 额定值 | 单位 | 测试方法 |
|---|---|---|---|
| 弯曲强度 (23°) | 400 | kgf/cm | ASTM D-790 |
| 弯曲弹性率 (80°) | 7000 | kgf/cm | ASTM D-790 |
| 屈服下的伸张强度 (-30°) | 1100 | kgf/cm | ASTM D-638 |
| 断裂下的延伸率 (23°) | >200 | % | ASTM D-638 |
| 屈服下的伸张强度 | 200 | kgf/cm | |
| 硬度(洛氏.布氏) (23°) | 55 | ASTM D-785 | |
| 弯曲强度 (80°) | 250 | kgf/cm | ASTM D-790 |
| 弯曲弹性率 (23°) | 25000 | kgf/cm | ASTM D-790 |
| Taber磨耗率 | 7 | mg | ASTM D-1044 |
| 屈服下的伸张强度 (80°) | 320 | kgf/cm | ASTM D-638 |
| 弯曲强度 (-30°) | 1400 | kgf/cm | ASTM D-790 |
| 断裂下的伸张强度 (23°) | >720 | kgf/cm | ASTM D-638 |
| 1%变形下的压缩强度 (23°) | 200 | kgf/cm | ASTM D-695 |
| 硬度(洛氏.布氏) (23°) | 85 | ASTM D-785 | |
| 1%变形下的压缩强度 (23°) | 100 | kgf/cm | ASTM D-695 |
| 屈服下的伸张强度 (80°) | 180 | kgf/cm | ASTM D-638 |
| 模压力 | 4700 | kgf/cm | |
| 抗冲击强度 (-30°) | 5.0 | kgf.cm/cm | ASTM D-256 |
| 弯曲强度 (-30°) | 1300 | kgf/cm | ASTM D-790 |
| 挤剪强度 (23°) | 650 | kgf/cm | ASTM D-732 |
| 屈服下的伸张强度 (-30°) | 870 | kgf/cm | ASTM D-638 |
| 弯曲强度 | ASTM D-790 | ||
| (23°) | 1100 | kgf/cm | |
| (80°) | 400 | kgf/cm | |
| 屈服下的伸张强度 (23°) | 750 | kgf/cm | ASTM D-638 |
| 屈服下的延伸率 (23°) | 8 | % | ASTM D-638 |
| 弯曲弹性率 (-30°) | 33000 | kgf/cm | ASTM D-790 |
| 屈服下的伸张强度 (23°) | 400 | kgf/cm | ASTM D-638 |
| 弯曲弹性率 (23°) | 7000 | kgf/cm | ASTM D-790 |
| 抗冲击强度 | ASTM D-256 | ||
| (23°) | 50 | kgf.cm/cm | |
| (23°) | 7.5 | kgf.cm/cm | |
| 硬度(洛氏.布氏) (23°) | 85 | ASTM D-785 | |
| 断裂下的伸张强度 | 780 | kgf/cm | |
| 弯曲弹性率 (80°) | 4000 | kgf/cm | ASTM D-790 |
| 硬度(洛氏.布氏) (23°) | 120 | ASTM D-785 | |
| 挤剪强度 (23°) | 600 | kgf/cm | ASTM D-732 |
| 弯曲弹性率 (-30°) | 35000 | kgf/cm | ASTM D-790 |
| 断裂下的伸张率 | 620 | % |
| 电气性能 | 额定值 | 单位 | 测试方法 |
|---|---|---|---|
| 介电损耗 (60HZ) | 0.01 | ASTM D-150 | |
| 绝缘耐力 | 20 | KV/mm | ASTM D-149 |
| 介电常数 (10HZ) | 3.5 | ASTM D-150 | |
| 介电损耗 | ASTM D-150 | ||
| (10HZ) | 0.12 | ||
| (10HZ) | 0.10 | ||
| 体积电阻率 | 10 | Ω.cm | ASTM D-257 |
| 介电损耗 (10HZ) | 0.02 | ASTM D-150 | |
| 介电常数 (10HZ) | 4.5 | ASTM D-150 | |
| 体积电阻率 | 10 | Ω.cm | ASTM D-257 |
| 介电常数 | ASTM D-150 | ||
| (10HZ) | 8.0 | ||
| (60HZ) | 3.9 | ||
| 介电损耗 (60HZ) | 0.10 | ASTM D-150 | |
| 介电常数 | ASTM D-150 | ||
| (60HZ) | 9.0 | ||
| (10HZ) | 3.8 | ||
| 介电损耗 (10HZ) | 0.02 | ASTM D-150 |
| 热性能 | 额定值 | 单位 | 测试方法 |
|---|---|---|---|
| 熔点 (DSC) | 215-225 | °C | |
| 线性热膨胀系数 | 8 | X的10-5cm/cm/°C | ASTM D-696 |
| 燃烧率 | V-2 | UL94 | |
| 热变形温度 | ASTM D-648 | ||
| (18.6kgf/cm) | 65 | °C | |
| (4.6kgf/cm) | 170 | °C |
| 其它性能 | 额定值 | 单位 | 测试方法 |
|---|---|---|---|
| 氧气 | 25 | me/m.24h |
PA6(聚已内酰胺#尼龙6)/1030B/泰国宇部
用途: V-2阻燃级 透明料 挤出级 高粘度 薄膜级 食品级。 特性备注:特性:高粘度 重要参数: 密度:1.14 g/cm3 吸水率:1.8 % 成型收缩率:1.2 % 断裂伸长率:200 % 弯曲强度:107.84 MPa弯曲模量:686.27 MPa 硬度:120 热变形温度:65 ℃ 生产厂商:日本宇部亚洲化学公司